Go Back  Bike Forums > Bike Forums > Long Distance Competition/Ultracycling, Randonneuring and Endurance Cycling
Reload this Page >

Is Galvanic corrosion a bigger problem with Generator bikes?

Notices
Long Distance Competition/Ultracycling, Randonneuring and Endurance Cycling Do you enjoy centuries, double centuries, brevets, randonnees, and 24-hour time trials? Share ride reports, and exchange training, equipment, and nutrition information specific to long distance cycling. This isn't for tours, this is for endurance events cycling

Is Galvanic corrosion a bigger problem with Generator bikes?

Old 11-28-20, 12:17 PM
  #1  
morrisond
Junior Member
Thread Starter
 
Join Date: Nov 2018
Location: Oakville, ON, Canada
Posts: 24

Bikes: The ones this month or last month?

Mentioned: 0 Post(s)
Tagged: 0 Thread(s)
Quoted: 10 Post(s)
Likes: 0
Liked 1 Time in 1 Post
Is Galvanic corrosion a bigger problem with Generator bikes?

I posted this in Electronics - but I figured the long distance crowd might have some experience with this if it is an issue. Just something that popped into my head.

I'm building a traditional Steel Rando bike. It will have an SON SL generator/light system where the current runs through the frame.

Does this worsen Galvanic Corrosion? Are Carbon Seatposts in Steel bikes a really bad idea with Generator Systems?

Thanks
morrisond is offline  
Old 11-28-20, 01:52 PM
  #2  
PaulH
Senior Member
 
Join Date: Jan 2002
Location: Washington, DC
Posts: 3,641
Mentioned: 3 Post(s)
Tagged: 0 Thread(s)
Quoted: 90 Post(s)
Liked 52 Times in 37 Posts
Been riding my generator bike through 20 years of salty winters with no obvious corrosion. They are much more durable than cars in my experience.
PaulH is offline  
Old 11-28-20, 01:56 PM
  #3  
unterhausen
Randomhead
 
Join Date: Aug 2008
Location: Happy Valley, Pennsylvania
Posts: 20,911
Mentioned: 0 Post(s)
Tagged: 0 Thread(s)
Quoted: 4 Post(s)
Liked 911 Times in 673 Posts
Galvanic corrosion doesn't really work that way. And I'm not sure there is going to be any extra potential between the seat post and frame, and their certainly will not be current flowing through the interface.

Are you running the taillight ground through the frame?

Mark the seatpost and take it out once a year, at least. Re-grease/carbon assembly paste and put it back in. Probably wouldn't be a bad idea to run a ball hone through the seat tube. Repeat every year.
unterhausen is offline  
Old 11-28-20, 02:27 PM
  #4  
Carbonfiberboy 
just another gosling
 
Carbonfiberboy's Avatar
 
Join Date: Feb 2007
Location: Everett, WA
Posts: 17,225

Bikes: CoMo Speedster 2003, Trek 5200, CAAD 9, Fred 2004

Mentioned: 106 Post(s)
Tagged: 0 Thread(s)
Quoted: 2840 Post(s)
Liked 745 Times in 559 Posts
Dissimilar metals immersed in an electrolyte solution generate their own potential between them as long as they are electrically connected which can be as simple as just touching. I don't think running a current through the frame changes the situation. I've had aluminum deteriorate on my carbon bike without a generator, just due to sweat, but carbon and aluminum are much further apart on the galvanic scale than are aluminum and steel. That said, it might be a good idea just to keep an eye on aluminum small parts, just in case. If they're shiny, they're fine. If they go all chalky, they are not fine. I doubt very much that it's a problem or we would have heard about it.
__________________
Results matter
Carbonfiberboy is offline  
Old 11-28-20, 02:38 PM
  #5  
morrisond
Junior Member
Thread Starter
 
Join Date: Nov 2018
Location: Oakville, ON, Canada
Posts: 24

Bikes: The ones this month or last month?

Mentioned: 0 Post(s)
Tagged: 0 Thread(s)
Quoted: 10 Post(s)
Likes: 0
Liked 1 Time in 1 Post
Thanks - just wanted to make sure as the SON SL system actually uses the bicycle frame as part of the circuit.
morrisond is offline  
Old 11-28-20, 05:09 PM
  #6  
unterhausen
Randomhead
 
Join Date: Aug 2008
Location: Happy Valley, Pennsylvania
Posts: 20,911
Mentioned: 0 Post(s)
Tagged: 0 Thread(s)
Quoted: 4 Post(s)
Liked 911 Times in 673 Posts
Rim dynamos used to have a grub screw on the frame clamp. There was no ground other than the frame, you screwed the grub screw through the paint into the tube. Many Shimano hub dynamo systems use the frame as ground too, the axle is ground. So using the frame as a conductor is nothing new, it's as old as dynamos. Which have been around longer than me.
unterhausen is offline  

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off


Thread Tools
Search this Thread

Contact Us - Archive - Advertising - Cookie Policy - Privacy Statement - Terms of Service - Do Not Sell My Personal Information -

Copyright 2021 MH Sub I, LLC dba Internet Brands. All rights reserved. Use of this site indicates your consent to the Terms of Use.