I don't have a taper attachment for my lathe. I...

I don't have a taper attachment for my lathe. I just turn the compound and crank it in and out by hand for short tapers like head tube cones.
Forum: Framebuilders
01-16-21, 05:17 AM
Replies: 34
Views: 3,497
Posted By dsaul

You can use the Furick cups with a 1/16 tungsten,...

You can use the Furick cups with a 1/16 tungsten, even though he doesn't recommend it. I ran 3/32 for a while, because I was switching back and forth between steel and aluminum and I didn't want to...
Forum: Framebuilders
11-27-20, 05:52 AM
Replies: 34
Views: 3,497
Posted By dsaul

20cfh is too high for an 8 cup with a gas lens. ...

20cfh is too high for an 8 cup with a gas lens. I stick with around 15cfh for an 8 cup, because any higher and the turbulence from the high flow causes it to pull atmospheric gases into the flow and...
Forum: Framebuilders
11-23-20, 02:06 PM
Replies: 34
Views: 3,497
Posted By dsaul

It seems to flow better than ER70S2 and I can use...

It seems to flow better than ER70S2 and I can use it for welding dissimilar metals like stainless dropouts to chromoly stays. Weldmold 880 is popular with framebuilders, but I believe that ER312 is...
Forum: Framebuilders
11-23-20, 01:40 PM
Replies: 34
Views: 3,497
Posted By dsaul

ER312 in .035 is what I use for all of my steel...

ER312 in .035 is what I use for all of my steel frames. The Furick Jazzy 10 is a good all around cup for framebuilding.
Showing results 1 to 5 of 5


 
Forum Jump

Contact Us - Archive - Advertising - Cookie Policy - Privacy Statement - Terms of Service - Do Not Sell My Personal Information -

Copyright 2021 MH Sub I, LLC dba Internet Brands. All rights reserved. Use of this site indicates your consent to the Terms of Use.