hi all how bout more info on product here it be
Silicon - Max 3.5%
Iron - Max 1.5%
Copper - 46-50%
Manganese - Max 1.5%
Zinc - Rem%
Tin - Max 3%
Silver - 5.8-6%
1690°F (921°C) 1715°F (935°C) AWS A5.8 RBCuZn-D