No blasting process with suffice, prior to plating. From my experience, working in a plating shop, the parts should be as shiny before plating, as you expect them to be, afterward. That's one reason that some platers will use a heavy copper plating first, to fill imperfections and minimize the loss of base material. Buffing the copper is a lot easier than buffing steel.