View Single Post
Old 08-04-17 | 01:40 PM
  #13  
howellhandmade
Senior Member
 
Joined: Apr 2014
Posts: 275
Likes: 0
From: Oakmont, PA
Originally Posted by 16Victor
I've seen his site but the contents are lost in the pile of other info in my head. I did desmut with nitric acid.

I'll try polishing, thanks.

AFA trying it - it's not trivial, but go for it!

Lucky for me, we do R&D on machining Ti, so I'll grab some from the scrap pile.
I meant to type, "NOT worth what he charges." I will give it a go, I just like to work out all the details before I jump. Handy on the titanium scrap, every place I've visited that machines titanium controls scrap pretty closely. I bought a variable DC power supply which, hopefully, will remove at least some guesswork. Did you start with battery acid before dilution, or a higher concentration? My plan is to use lye to de-smut, dealing with one type of acid bath is enough.
howellhandmade is offline  
Reply