Originally Posted by
wesmamyke
Interesting tube damage there. That's a bonded steel/aluminum one right?
Yeah... one wonders if the differences in how the frame was constructed, as compared to a conventional steel lugged frame, has pushed the yield point further back along the length of the tubes. It's interesting too that the bond didn't fail before the tube yielded (good to know).